Manufacturing
Jewelry manufacturing process: CAD, lost-wax casting, hallmark
By Siona Jewels team · · 11 min read

Short answer
A jewellery order moves from brief to CAD, then a printed resin or injected wax pattern, lost-wax casting, finishing, setting, polishing, quality control and hallmarking. Buyers sign off the CAD and a sample, and the later stages decide whether production matches it. In India, BIS hallmarking with a six-digit HUID is mandatory in 392 districts as of August 2026.
A quote for a ring is really a quote for more than a dozen steps, each with its own way of going wrong. Once you know the sequence, a lot makes sense. You can see why a sample takes the time it does, and why a design change after the mould is made costs more than one at CAD. You can also tell where a pitted shank or a loose stone came from.
This guide follows one order from brief to hallmark, the way it moves through a Mumbai workshop. It doesn't give a duration for each stage, because those depend on the design and the run. For timings, see the custom jewellery production timeline.
What are the main stages of the jewellery manufacturing process?
Fine jewellery with settings and detail is usually cast by the lost-wax method, then finished, set, polished, checked and hallmarked. A 2019 paper on investment casting by Ulrich Klotz and colleagues at fem sets out the core sequence: wax models injected or printed, invested, burned out overnight, cast, quenched and cut from the tree. The table shows what you approve along the way.
Stage | What happens | What the buyer approves or checks |
|---|---|---|
| Design, metal, stones, sizes and quantities fixed | Written specs, including stamping |
| Measured 3D model built | Renders, dimensions, stone layout |
| Model printed in castable resin or wax | Optional printed proof for scale |
| Rubber mould made; wax copies injected for runs | Master sample, before the mould |
| Patterns sprued to a tree; flask filled | None; faults show at QC |
| Kiln removes pattern, cures mould | None; faults show at QC |
| Molten metal fills the cavity | Metal and karat as ordered |
| Investment removed; pieces cut off | None |
| Sprue stubs removed, surfaces refined | Finish against the sample |
| Stones set | Security, alignment, melee match |
| Final polish; rhodium if specified | Colour and finish against the sample |
| Weights, measurements, stones, finish | QC photos and weights |
| BIS hallmark (India); quality mark plus trademark (US) | Mark content and placement |
| Lab reports matched to stones | Report numbers against inscriptions |
What happens at the CAD stage, and what should you approve?
CAD turns the brief into a measured 3D model, and it's the cheapest place to change anything. Common tools include Rhino and jewellery plug-ins that run on it. MatrixGold 4.0, Gemvision's jewellery software built on Rhino, was released in May 2026. You approve renders and dimensions here, before any metal is used.
Ask for renders from several angles plus a dimensioned view. Check the finger size, the band width and thickness at its narrowest point, the stone sizes and layout, and the prong count. Check the gallery height and how the piece will sit on a finger or an ear. If the piece needs a quality stamp, agree where it goes now, so the model leaves a flat area for it.
The model also drives the price. Software can estimate metal weight from the model's volume, which is how a quote for a 10 g 18K ring gets its gold figure before anything is cast. 18K is 750 parts per thousand, so that ring contains 7.5 g of fine gold (10 × 0.750). The cost breakdown guide shows how that weight becomes a price. Changes after sign-off cost more, because every later stage builds on the approved model.
How are wax and resin patterns made?
There are two routes. For first samples and one-offs, the CAD file is 3D-printed in castable resin or wax. For repeat production, a master is moulded in rubber and wax copies are injected into the mould, as Klotz's paper describes. Formlabs' instructions call for printed castable resin to be post-cured for 4 hours at 60 °C.
Printed patterns reproduce the CAD exactly, fine detail included, and need no mould. That's why samples and bridal one-offs are usually printed. Each print is destroyed in casting, though, so every piece needs its own.
For a range, the workshop makes a metal master from the approved sample, builds a rubber mould around it and injects wax for each copy. Injection is quicker per piece on a run. The catch is that the mould fixes the design, so any change means a new master and a new mould. Approve the master sample with that in mind: on a 50-piece order, every one of the 50 waxes comes out of that mould.
How does lost-wax casting work?
Patterns are attached to a central wax sprue to form a tree, which stands in a steel flask filled with investment: gypsum-bonded or phosphate-bonded silica, depending on the metal. A kiln burns the pattern out overnight, metal fills the cavity, and the investment is broken away. Klotz describes this sequence for platinum.
Treeing and investing
Where each pattern joins the tree, and how thick that sprue is, decides how metal flows in and how the piece shrinks as it cools. Spruing is a skilled job, and it comes back in the porosity section below. Once the tree is built, the flask goes on, investment slurry is poured around the tree and left to set.

Burnout: wax and resin need different cycles
For wax, a burnout guide by Calloway, published on Ganoksin, sets a first step at no more than 149 °C (300 °F) for at least 30 minutes. A cure up to 732 °C (1,350 °F) follows. The guide warns never to go to 816 °C (1,500 °F), because gypsum investment breaks down there. The flask then holds at casting temperature for at least an hour.
Castable resin needs its own cycle, which takes about 13 hours to reach casting temperature on Formlabs' standard schedule. It ramps to 177 °C over 150 minutes and holds for 30, then ramps over 270 minutes to 732 °C and holds there for 180, before cooling to about 482 °C. The heating and holds alone take 630 minutes (150 + 30 + 270 + 180), or 10.5 hours. When samples are printed and production is injected, it's fair to ask whether each goes through the right cycle.
Casting: vacuum, centrifugal and platinum
Molten metal enters the hot mould by gravity, by tilting with vacuum or gas-pressure assistance, or driven in by a spinning centrifugal arm. Platinum is the most demanding. In Klotz's work, platinum flasks were preheated to 500–900 °C, usually 850 °C, and simulated melts ran at 1,850–1,980 °C. Platinum-ruthenium (950) needed at least 100 K of superheat and platinum-cobalt 50–80 K. Centrifugal casting filled moulds better than tilt casting. That's one reason platinum work is quoted differently from gold.
Devesting and cutting off
The hot flask is quenched in water, which breaks up the investment. What's left comes off under a water jet or glass-bead blasting, and each piece is cut from the tree, per Klotz. Castings come out dull, with a sprue stub on every piece.

What causes porosity in cast jewellery, and how is it prevented?
Porosity means small voids in or under the metal surface. A 1987 Santa Fe Symposium paper called it the most common casting problem, and it's still what buyers find when a polished shank shows pinholes. Two causes matter most: shrinkage, when metal freezes in the wrong order, and investment that breaks down in the kiln.
Shrinkage. Metal shrinks as it solidifies, and a section that freezes last needs liquid metal to keep feeding it. Klotz explains that sprues should be placed so solidification runs from the tip of the part back towards the sprue. Picture a ring with a heavy head and a thin shank, sprued at the shank. The shank freezes first, the head is cut off from its supply, and voids form inside it.
Investment breakdown. Overheat gypsum investment during burnout, past the 816 °C limit in the Ganoksin guide, and the mould itself degrades. The result is rough, pitted surfaces. That's why burnout cycles are written down and followed.
The standard reference on these faults is Dieter Ott's Handbook on Casting and Other Defects in Gold Jewellery Manufacture (World Gold Council, 1997). For a buyer, the practical step is simpler. Reject pitting at the sample stage, and ask how the workshop spots porosity before polishing hides it.
Is every piece cast, or are some die-struck?
Not every piece is cast. Die-striking presses solid metal between hardened steel dies instead of pouring it, so it avoids casting porosity altogether. It suits simple, repeatable shapes such as plain bands and some findings. Detailed pieces with stone settings and undercuts are usually cast.
The trade-off is tooling: dies are cut for one shape, so striking makes sense for long runs of a single design rather than a varied range.
What happens after casting: filing, setting, polishing and plating?
The rough casting is filed and pre-polished, the stones are set, the piece gets its final polish, and white gold is usually rhodium-plated. This is the hand-work stage, and it's where the approved sample earns its keep. Each step is checked against it, and most visible defects get caught or missed here.
Filing removes the sprue stub and casting skin. Pre-polishing comes before setting, because polishing tight corners is much harder once stones are in. The common setting styles each have their own checks:
- Prong (claw): metal tips are bent over the stone's girdle. Each tip should cover the edge and none should snag.
- Pavé: small stones sit close together in drilled seats, held by tiny beads raised from the metal. Rows should be even, with no stone sitting proud.
- Bezel: a metal rim wraps the whole girdle. It should be tight all round, with no gap.
- Channel: stones sit between two parallel walls. The walls should run straight and no stone should rattle.
White gold is often rhodium-plated for a whiter colour. The plating wears with use and can be renewed, so say on the order whether white gold pieces are plated. Final QC compares each piece with the sample for weight, measurements, stone security, stamp and finish. For which karats suit which market, see gold karat by market.
How is jewellery hallmarked for India and stamped for the US?
In India, gold jewellery carries a BIS hallmark: the BIS logo, a purity mark such as 22K916, 18K750 or 14K585, and a six-digit HUID laser-marked at a hallmarking centre, according to BIS. It's mandatory in 392 districts as of August 2026. In the US, 15 U.S.C. §297 requires anyone who applies a gold quality mark such as "14K" to add their own trademark or name next to it.
India: the BIS hallmark and HUID
The six-digit HUID has been part of the hallmark since 1 July 2021. Mandatory hallmarking started in 256 districts on 23 June 2021. The sixth phase, on 2 March 2026, took it to 380 districts, All India Radio News reported, and more than 60 crore items carried an HUID by March 2026. A seventh phase on 28 April 2026 took it to 385 districts, and an eighth on 3 August 2026 added seven more, for 392 in all, according to BIS's phase-wise district list. The list keeps growing, so check it when you plan an India launch.
BIS also lists exemptions. They include exports made to a foreign buyer's specification, articles under 2 g, jewellers with turnover up to ₹40 lakh, Kundan, Polki and Jadau work, and pieces for international exhibitions. So pieces made for export to a US, Canadian or UAE buyer's specification don't need the BIS hallmark; that market's marking rules apply instead.
US: quality mark plus trademark
Under §297, whoever applies a quality mark must also apply their trademark or name, by the same method, at least as large and as close to it as possible. The decision for a private-label buyer is whose mark goes on the piece, yours or the manufacturer's, and where it sits. Siona Jewels supplies BIS-hallmarked gold for India and trademark-stamped pieces for the US and Canada. Whoever you work with, put the stamp specification in the brief so CAD leaves room for it.
Where does centre-stone certification fit in the process?
Labs grade centre stones loose, so certification happens before setting, and the report travels with the finished piece. The checkpoint for the buyer comes at the end, when the report number is matched against the inscription on the stone's girdle. Lab-grown centres need extra attention to the type of report and the disclosure wording.
Both are covered in the lab-grown diamond jewellery wholesale checklist. For natural stones, the logic is the same: agree the lab, get report copies before dispatch, and spot-check inscriptions on arrival.
Why is so much jewellery made in Mumbai's SEEPZ?
Mumbai's SEEPZ special economic zone accounted for nearly half of India's SEZ jewellery exports. GJEPC's SEZ booklet puts SEEPZ exports at US$3.36 billion in FY2022-23, 46.74% of all gem and jewellery exports from India's SEZs. Studded gold jewellery made up US$2.57 billion of that, and 63.98% of it went to the US.
Studded gold was 76.52% of SEEPZ's exports (US$2,572.93 million ÷ US$3,362.55 million). Against India's US$38.11 billion in gem and jewellery exports that year, SEEPZ alone was about 8.8% (3.36 ÷ 38.11). For a buyer, the point is that the zone's main product is studded gold made for the US market. The booklet's annexure adds provisional FY2023-24 figures: SEEPZ exported US$3.37 billion, 52.6% of SEZ gem and jewellery exports, and studded gold made up 80.5% of that.
What to do next
Get each sign-off in writing: brief, CAD, sample, then production. Before you approve the CAD, settle four things: printed or moulded patterns, metal and karat, stamping, and plating. Ask how the workshop checks for porosity, and keep the approved sample as the master for QC. If you're sourcing from India for the first time, read how to source private-label jewellery from India. When your designs and quantities are ready, send a brief.
Planning a range?
Send us your designs, metals and quantities, and we’ll reply with a quote and timeline within one business day.
Questions buyers ask
Only if your contract says so. Agree it before CAD starts. Cover who owns the CAD file and the rubber moulds, whether the manufacturer may reuse the design, and what happens to moulds if you move production. For private-label ranges, ask for the CAD files to be released to you on full payment.
Not under the mandatory scheme, as of October 2026. The BIS grades are 14, 18, 20, 22, 23 and 24K, with 9K voluntary; 10K isn't listed. 10K made in India for export to a buyer's specification falls under the export exemption, and in the US it carries a quality mark and trademark instead.
Hot isostatic pressing (HIP) treats a finished casting with high heat and gas pressure together. Klotz's 2019 paper notes it can remove micro-shrinkage porosity in platinum castings. It's an extra process step, so ask whether it's included when a platinum quote looks different from another workshop's.
Yes. Ask for a printed resin proof once the CAD is approved. It shows scale, proportion and how a ring or earring sits, at little cost compared with a metal sample. It won't show metal colour, finish or stone sparkle, so use it to judge size and shape only.
It depends on the design, quantity and whether a mould is needed. Our [production timeline guide](/guides/custom-jewellery-production-timeline) puts brief to dispatch at 4–8 weeks. Sign-offs on CAD and samples are the part of that schedule a buyer controls, so turn them around quickly and in writing.